Research Article
Passivity and Semiconducting Behavior of a High Nitrogen Stainless Steel in Acidic NaCl Solution
Figure 7
ARXPS component analyses of HNSS surface after passivation at 0 V (SCE) for 90 min in 0.05 M H2SO4 + 0.5 M NaCl after sputtering time for 10 s.