Research Article
On the Development of an Al4.8 wt% Cu Alloy Obtained from Recycled Aluminum Cans Designed for Thixoforming Process
Figure 9
Microstructure of samples thixoforged of the Al4.8 wt% Cu alloy (a) and resting time 20 min, (b) and resting time 30 min, (c) and resting time 20 min, (d) and resting time 30 min, and (e) and resting time 20 min without etching.
(a) |
(b) |
(c) |
(d) |
(e) |