Mix proportion for GPC.

Mineral admixtureChemical admixtureCoarse aggregate
(kg/m3)
Fine aggregate
(kg/m3)
MolarityCuring temperatureSuperplasticizers
Fly ashGGBSNaOHNa2SiO3
kg/m3kg/m3kg/m3kg/m3

257.16171.4448.97122.43126054012 M60°2% of binder