Research Article

The Static and Dynamic Mechanical Properties of Magnetorheological Silly Putty

Table 5

, , AMRe, and RMRe% of MRSP-4 with externally applied magnetic field at different temperatures.

Temperature/MPa/MPaAMRe/MPaRMRe%

10°C2.170.7541.416187.80%
20°C1.590.4221.168276.78%
40°C1.250.1091.1411046.79%
60°C1.010.002421.0075841635.54%