Research Article
Study on Strength and Microstructure of Cement-Based Materials Containing Combination Mineral Admixtures
Table 6
Contribution rates of the hydration activity effect.
| Samples | 3 d | 7 d | 28 d | 90 d |
| GL1 | −0.15 | −0.14 | −0.16 | −0.03 | GL2 | −0.25 | −0.17 | −0.34 | 0.03 | GL3 | −0.21 | −0.40 | −0.16 | 0.17 | GS1 | −0.03 | 0.08 | −0.06 | 0.06 | GS2 | −0.12 | −0.13 | −0.18 | 0.03 | GS3 | −0.15 | −0.25 | −0.12 | 0.06 | LS1 | 0.26 | 0.17 | 0.03 | 0.16 | LS2 | 0.18 | 0.31 | 0.01 | 0.18 | LS3 | 0.10 | 0.13 | −0.03 | 0.12 | GLS1 | 0.15 | 0.18 | 0.06 | 0.13 | GLS2 | 0.04 | 0.05 | 0.05 | 0.09 | GLS3 | 0.05 | −0.01 | −0.05 | 0.00 |
|
|