Research Article
Effect of Mg Content and Heat Treatment on the Mechanical Properties of Low Pressure Die-Cast 380 Alloy
Figure 16
Fracture surfaces of DCM5 fatigue samples: (a, b, and d) after casting and (c) after aging at 220°C for 25 h.
(a) |
(b) |
(c) |
(d) |