Research Article

Experimental and Numerical Study of Mild Steel Behaviour under Cyclic Loading with Variable Strain Ranges

Table 1

Chemical composition of liquid alloys of S275 and S355 (%).

Steel gradeCMnSiPSNCuNiCrMoVAlTiNb

EN 10025 standardS275<0.18<1.5<0.55<0.03<0.03<0.012<0.55
S355<0.2<1.6>0.14<0.03<0.03<0.012<0.55
<0.25

Measured valueS2750.1731.020.0210.0160.0050.00510.0080.0120.0140.0010.0010.050.0010.001