Research Article
Using Recycled Glass and Zeolite in Concrete Pavement to Mitigate Heat Island and Reduce Thermal Cracks
Table 5
Mixture proportions of mortar bars.
| Mixtures | Cement (gr) | Water (gr) | Fine aggregate (gr) | Zeolite (gr) | Recycled glass (gr) |
| Control mixture | 440 | 207 | 990 | — | — | G10Z0 | 440 | 207 | 900 | — | 90 | G10Z10 | 396 | 207 | 900 | 44 | 90 | G10Z30 | 308 | 207 | 900 | 132 | 90 | G20Z0 | 440 | 207 | 800 | — | 200 | G20Z10 | 396 | 207 | 800 | 44 | 200 | G20Z30 | 308 | 207 | 800 | 132 | 200 | G30Z0 | 440 | 207 | 600 | — | 300 | G30Z10 | 396 | 207 | 600 | 44 | 300 | G30Z30 | 308 | 207 | 600 | 132 | 300 |
|
|