Influence of Deposition Condition on Y2O3 Coatings Produced by Pulsed Electrophoretic Deposition
Figure 4
Surface SEM images of films deposited at various bias frequencies (10 Hz, 1 kHz, and 100 kHz), with bias voltage of 0.5 V and Y2O3 concentration of 0.5 wt% in a suspension solution.
(a) |
(b) |
(c) |