Influence of Deposition Condition on Y2O3 Coatings Produced by Pulsed Electrophoretic Deposition
Figure 6
Surface SEM images of the films deposited at various bias voltages (0.5, 2.0, and 5 V), with bias frequency of 1 kHz and the Y2O3 concentration of 0.5 wt% in a suspension solution.