Research Article
Evaluation of a Cold-Mixed High-Performance Polyurethane Mixture
Table 5
Results of the Hamburg wheel tracking tests.
| Mixture | VV (%) | Creep slope (×10−3) | Stripping slope (×10−3) | Rutting depth (mm) | SIP (×103) |
| PUM | 1-1 | 19.75 | −0.02 | — | 0.73 | — | 1-2 | 19.81 | −0.02 | — | 0.85 | — | SMA | 2-1 | 3.83 | −0.2 | −0.3 | 7.28 | 15 | 2-2 | 3.84 | −0.2 | −0.3 | 5.97 | 15 |
|
|