Research Article
Effect of Heat Treatment and Titanium Addition on the Microstructure and Mechanical Properties of Cast Fe31Mn28 Ni15Al24.5Tix High-Entropy Alloys
Figure 10
SEM and the corresponding point analysis at different positions for the C3 sample after heat treatment at 900°C for 10 h.