Research Article
Factors Influencing the Rheological Properties of MRSP Based on the Orthogonal Experimental Design and the Impact Energy Test
Table 1
The major performance indexes of CIP.
| Fe content | C content | O content | N content | Average particle size | Apparent density | Tap density |
| 98.030% | 0.730% | 0.276% | 0.964% | 3.500 μm | 2.800 g·cm−3 | 4.200 g·cm−3 |
|
|