Three-Point Bending Fatigue Test of TiAl6V4 Titanium Alloy at Room Temperature
Figure 10
Striation (a) in a perpendicular direction to fatigue crack propagation and secondary fatigue cracks (b) parallel to the advancing crack front, SEM.