Research Article
Three-Point Bending Fatigue Test of TiAl6V4 Titanium Alloy at Room Temperature
Figure 8
Initiation sites of fatigue crack on the free surface: (a) spec. no. 9, (b) spec. no. 7. Cleavage facets made by transcrystalline cleavage failure of the TiAl6V4 alloy grain at the fatigue crack initiation sites: (c) spec. no. 9; (d) spec. no. 7, details of the initiation site, SEM.
(a) |
(b) |
(c) |
(d) |