Research Article

Semisolid Compression Brazing of Al50Si Alloy Using Zn-Al-Cu Filler Metal Assisted by SiC Particles

Figure 4

Interfacial microstructure of the joint with 5 μm SiC particles at (a) 1 g/m2, (b) 3 g/m2, (c) 7 g/m2, (d) 16 g/m2, and (e) and (f) 32 g/m2.
(a)
(b)
(c)
(d)
(e)
(f)