Research Article
Mechanical Recovery of Cracked Fiber-Reinforced Mortar Incorporating Crystalline Admixture, Expansive Agent, and Geomaterial
Table 5
Water flow rate and self-healing indices of the three mixes.
| Mix type | Crack width (μm) | Water flow (ml·mm−1·min−1) | Self-healing index (%) | | |
| OPC-28D-227 | 227 | 0.68 | 0.19 | 72.4 | OPC-28D-241 | 241 | 0.89 | 0.30 | 66.0 | OPC-28D-250 | 250 | 1.06 | 0.40 | 63.0 | SH1-28D-221 | 221 | 0.75 | 0.12 | 84.3 | SH1-28D-230 | 230 | 0.90 | 0.16 | 82.2 | SH1-28D-247 | 247 | 1.00 | 0.18 | 81.9 | SH2-28D-225 | 225 | 0.74 | 0.06 | 91.9 | SH2-28D-238 | 238 | 0.81 | 0.09 | 89.3 | SH2-28D-251 | 251 | 1.01 | 0.11 | 88.7 |
|
|