EDS analysis results of mortar crack surfaces.

Mix typeCOKSiNaAlCaOtherTotal

OPC21.850.20.42.724.40.5100
SH120.328.90.919.22.628.10.0100
SH214.630.20.611.73.74.234.90.1100