Research Article
Minimum Water Requirement Method for High-Performance Sulphoaluminate Cement-Based Materials
Table 3
Mix ratios of compound cement paste.
| Dosage (%) | Test No. | Cement | Fly ash | Silica fume | Steel slag | Water binder ratio | Water reducing agent |
| A1 | 86.5 | 4 | 5 | 4.5 | 0.27 | 0.6 | A2 | 77 | 4 | 10 | 9 | 0.27 | 0.6 | A3 | 67.5 | 4 | 15 | 13.5 | 0.27 | 0.6 | A4 | 80 | 6 | 5 | 9 | 0.27 | 0.6 | A5 | 70.5 | 6 | 10 | 13.5 | 0.27 | 0.6 | A6 | 74.5 | 6 | 15 | 4.5 | 0.27 | 0.6 | A7 | 67.5 | 8 | 5 | 13.5 | 0.27 | 0.6 | A8 | 77.5 | 8 | 10 | 4.5 | 0.27 | 0.6 | A9 | 68 | 8 | 15 | 9 | 0.27 | 0.6 |
|
|