Orthogonal test analysis.

Functionā€‰Dosage (%)
FFSSSF

Standard consistencyK11.1721.0491.027
K21.1281.1511.17
K31.1511.2511.254
R0.0440.2020.227

Strength after 28ā€‰dK1229.9238.6228
K2239.3236.0239.6
K3202.5197.1204.1
R36.5541.4435.64