Research Article

Selective Laser Melting of Diamond-Containing or Postnitrided Materials Intended for Impact-Abrasive Conditions: Experimental and Analytical Study

Figure 7

Digital photos of manufactured Ti6Al4V lattice (a) and heated and nitrided Ti6Al4V lattices at 750°C (b), 900°C (c), and 1050°C (d). Volume fraction and unit cell size are 6% and 2 mm, respectively (diameter of lattice structures is 20 mm, and length is 15 mm).