Research Article
Microstructure and Mechanical Properties of the Cold-Rolled Mg-14Li-1Zn Alloy after Hot Rolling
Figure 3
TEM images of the cold-rolled specimen after hot rolling under different temperatures. (a, b) 100°С; (c, d) 150°С; (e, f) 200°С; (g, h) 250°С; (i, j) 300°С.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |
(h) |
(i) |
(j) |