Research Article
Microstructure and Mechanical Properties of the Cold-Rolled Mg-14Li-1Zn Alloy after Hot Rolling
Table 1
Tensile testing values from Figure
5.
| Temperature (°C) | Ultimate tensile strength (MPa) | Elongation (%) |
| 100 | 179 | 11.9 | 150 | 204 | 22.9 | 200 | 196 | 24.6 | 250 | 220 | 16.3 | 300 | 238 | 14.2 |
|
|