Research Article
Influence of Hydrogen Content on the Microstructure and Mechanical Properties of ER5183 Wires
Figure 7
The fracture morphology of the ϕ5.2 mm wire with hydrogen content of 0.26 μg/g. (a) Macroscopic morphology of the fracture; (b) and (c) microscopic view of the internal cracks; (d) schematic diagram of the H-rich zone and internal cracks.
(a) |
(b) |
(c) |
(d) |