Advances in Materials Science and Engineering / 2019 / Article / Tab 5

Research Article

Impact of High-Velocity Oxy-Fuel ZrO2 Coating on Corrosion Resistance and Fatigue Life of AISI 316L Austenitic Stainless Steel

Table 5

Fatigue life (cycles) of uncoated AISI 316L austenitic stainless steel specimen.

S. no.Test conditionFatigue life (cycles)
Stress (MPa)Strain amplitude (%)Strain rateTrial 1Trial 2

12500.43 × 10−3 s−11122711212

We are committed to sharing findings related to COVID-19 as quickly and safely as possible. Any author submitting a COVID-19 paper should notify us at help@hindawi.com to ensure their research is fast-tracked and made available on a preprint server as soon as possible. We will be providing unlimited waivers of publication charges for accepted articles related to COVID-19. Sign up here as a reviewer to help fast-track new submissions.