Concrete mixture proportions (kg/m3).
| Specimens | w/b | Cement | Water | Sand | Natural aggregates | SR |
| C-ISR-0% SR | 0.5 | 320 | 160 | 653 | 1267 | 0 | C-ISR-1% SR | 157.8 | 3.2 | C-ISR-2% SR | 155.5 | 6.4 | C-ISR-3% SR | 153.3 | 9.6 | C-ISR-4% SR | 151 | 12.8 |
|
|