Influence of Water-Repellent Treatment with Silicon Resin on Properties of Concrete
Table 3
Capillary water absorption coefficient and decrease rate of C-ISR and C-SSR.
| Amount of added SR | Plain | 1% | 2% | 3% | 4% | 100 g/m2 | 200 g/m2 | 300 g/m2 | 400 g/m2 | 600 g/m2 |
| Capillary absorption coefficient | 523.4 | 450.5 | 384.0 | 285.6 | 282.4 | 205.2 | 131.1 | 124.3 | 64.4 | 43.4 | Decrease rate (%) compared to plain concrete | — | 13.9 | 26.6 | 45.4 | 46.0 | 60.8 | 75.0 | 76.3 | 87.7 | 91.7 |
|
|