Research Article

Elastic-Plastic Behavior of Compacted Loess under Direct and Cyclic Tension

Figure 4

Direct tensile test σ × ε curves at different water contents: (a) ρd = 1.55 g/cm3; (b) ρd = 1.65 g/cm3.
(a)
(b)