Research Article
Study on the Process Optimization and Wear Resistance of Electron Beam Cladding WC-CoCr Coating on Inconel 617 Surface
Table 3
Cladding orthogonal experiment of WC-CoCr.
| Number | Factor | A (mA) | B (Hz) | C (kV) | D (mm) | E (%) | F (mm/min) |
| 1 | 80 | 500 | 50 | 8 | 2 | 800 | 2 | 80 | 500 | 50 | 8 | 4 | 1000 | 3 | 80 | 500 | 50 | 8 | 6 | 1200 | 4 | 80 | 550 | 55 | 9 | 2 | 800 | 5 | 80 | 550 | 55 | 9 | 4 | 1000 | 6 | 80 | 550 | 55 | 9 | 6 | 1200 | 7 | 80 | 600 | 60 | 10 | 2 | 800 | 8 | 80 | 600 | 60 | 10 | 4 | 1000 | 9 | 80 | 600 | 60 | 10 | 6 | 1200 | 10 | 83 | 500 | 55 | 10 | 2 | 1000 | 11 | 83 | 500 | 55 | 10 | 4 | 1200 | 12 | 83 | 500 | 55 | 10 | 6 | 800 | 13 | 83 | 550 | 60 | 8 | 2 | 1000 | 14 | 83 | 550 | 60 | 8 | 4 | 1200 | 15 | 83 | 550 | 60 | 8 | 6 | 800 | 16 | 83 | 600 | 50 | 9 | 2 | 1000 | 17 | 83 | 600 | 50 | 9 | 4 | 1200 | 18 | 83 | 600 | 50 | 9 | 6 | 800 | 19 | 85 | 500 | 60 | 9 | 2 | 1200 | 20 | 85 | 500 | 60 | 9 | 4 | 800 | 21 | 85 | 500 | 60 | 9 | 6 | 1000 | 22 | 85 | 550 | 50 | 10 | 2 | 1200 | 23 | 85 | 550 | 50 | 10 | 4 | 800 | 24 | 85 | 550 | 50 | 10 | 6 | 1000 | 25 | 85 | 600 | 55 | 8 | 2 | 1200 | 26 | 85 | 600 | 55 | 8 | 4 | 800 | 27 | 85 | 600 | 55 | 8 | 6 | 1000 |
|
|