Research Article
Investigation of the Performance of the Ecofriendly Fiber-Reinforced Asphalt Mixture as a Sustainable Pavement Material
Table 1
Technical indicators of the asphalt binder.
| Test properties | Unit | Test results | Test basis |
| Penetration (25°C, 100 g, 5 s) | 0.1 mm | 86.4 | ASTM D5-97 | Softening point | °C | 47.0 | ASTM D36-06 | Ductility (15°C, 5 cm/min) | cm | 182 | ASTM D113-99 | Wax content | % | 1.74 | ASTM D3344-90 | Specific gravity | — | 1.030 | ASTM D70-76 | Flash point | °C | 304 | ASTM D92-02 |
| RTFOT (163°C, 75 min) |
| Mass change | % | 0.15 | ASTM D2872-04 | Penetration ratio (25°C) | % | 60.5 | ASTM D5-97 | Ductility (10°C) | cm | 10.1 | ASTM D113-99 |
|
|