Research Article

Effect of Grain Size and Film Thickness on the Thermoelectric Properties of Flexible Sb2Te3 Thin Films

Figure 1

XRD spectra of Sb2Te3 thin films fabricated under different deposition times: 15, 30, 45, and 60 min.