Research Article
Fretting Wear Behavior and Damage Mechanisms of Inconel X-750 Alloy in Dry Contacts
Figure 4
Superimposed cross-section profiles of wear scars perpendicular to the fretting direction through fretting time. (a) After 10 minutes. (b) After 30 minutes. (c) After 90 minutes.
(a) |
(b) |
(c) |