Mineral composition of loess and treated loess samples.
| Samples | Hornblende (%) | Gypsum (%) | Quartz (%) | Feldspar (%) | Calcite (%) | Pyroxene (%) | Kaolin (%) |
| MZS-0 | 4.20 | 1.19 | 35.50 | 16.80 | 11.87 | 5.00 | 25.44 | MZS-1 | 4.33 | 1.40 | 32.84 | 17.65 | 12.27 | 5.40 | 26.11 | MZS-2 | 5.12 | 1.20 | 32.68 | 18.24 | 8.42 | 6.10 | 28.24 | MZS-3 | 6.14 | 1.77 | 30.82 | 18.20 | 5.48 | 6.33 | 31.26 | MZS-4 | 6.00 | 1.65 | 30.71 | 19.55 | 0.79 | 7.85 | 33.45 |
|
|