Experimental Study on Electrode Wear of Diamond-Nickel Coated Electrode in EDM Small Hole Machining

Table 6

Physical properties of materials.

MaterialMelting point (°C)Specific heat capacity (J/g·K)Coefficient of thermal conductivity (W/m·K)Electrical conductivity (S/m)Work function (eV)

Brass967377108.91.67 × 1073.34–5.24
Copper1083386386.45.95 × 1075.24
Copper-tungsten alloy3000–34102202.5 × 1074.54–5.24
Molybdenum26202551421.93 × 1064.37
Nickel1453452.259.21.43 × 107
Diamond3550399–4722000Almost nonconductive