Research Article
Effect of Sterilization on the Properties of a Bioactive Hybrid Coating Containing Hydroxyapatite
Figure 6
DRX of the coating before and after sterilization immersed for 24 and 672 hours in SBF at 37 ± 3°C: (a) Ti6Al4V/TM/TMHA, (b) Ti6Al4V/TM/TMHA/OE, (c) Ti6Al4V/TM/TMHA/AC, and (d) Ti6Al4V/TM/TMHA/PH.
(a) |
(b) |
(c) |
(d) |