Research Article

Brazeability, Microstructure, and Joint Characteristics of ZrO2/Ti-6Al-4V Brazed by Ag-Cu-Ti Filler Reinforced with Cerium Oxide Nanoparticles

Figure 8

The cross-sectional SEM image of the ZrO2/Ti-6Al-4V interface brazed using various Ag-Cu-Ti-xCeO2 composites: (a) x = 0; (b) x = 0.03; (c) x = 0.05; (d) x = 0.1; (e) EDS analysis of (d).
(a)
(b)
(c)
(d)
(e)