EDS data of different phases in Figures 5(b)–5(d).

Serial no.Sample IDCu (at.%)Ag (at.%)Ti (at.%)Phase

1Point 136.4163.59Ag-Cu
2Point 2100.000Cu
3Point 331.721.4866.8Cu2Ti