Research Article
Effect of Isothermal Treatment on Microstructure and Mechanical Properties of Cold-Deformed IF Steel
Figure 6
Stress-strain curves obtained for IF steel as a function of different recrystallisation times in the ranges (a) 0–180 s and (b) 240–420 s at a temperature of 780°C.
(a) |