Research Article
Directional Solidification of Sn-Cu6Sn5 In Situ Composites
Figure 1
Sn-0.7 wt.% Cu samples directionally solidified and grown from right to left. V = 0.5 µm/s; GL = 2.5 K/mm. Longitudinal view of (a) (ηP + Liq) + Liq. interface at the top of growth; (b) solid + (ηP + Liq) interface.
(a) |
(b) |