Composition of mortars.

MixCement (kg/m3)MgO (kg/m3)Water (kg/m3)Sand (kg/m3) ratio

CM560.7ā€”280.31406.90.50
MA10504.656.1280.31406.90.50
MA15476.684.1294.31406.90.52
MA20448.5112.1304.31406.90.54
MG10504.656.1280.31406.90.50
MG15476.684.1342.31406.90.61
MG20448.5112.1342.31406.90.61