Research Article
Material and Structural Properties of Fiber-Reinforced Resin Composites as Thin Overlay for Steel Bridge Deck Pavement
Figure 15
Bending test results at low temperature. (a) Bending and tensile strength at −10°C; (b) the maximum bending and tensile strain at −10°C; (c) bending stiffness modulus at −10°C.
(a) |
(b) |
(c) |