Research Article
Effects of Cryogenic Treatment and Tempering on Mechanical Properties and Microstructure of 0.25C-0.80Si-1.6Mn Steel
Figure 8
DCT at −110°C and tempering at 350°C. (a) Misorientation histogram of grain, (b) image of grain size, (c) misorientation histogram of FCC, and (d) misorientation histogram of BCC.
(a) |
(b) |
(c) |
(d) |