Research Article

High Frequency Vibration Fatigue Behavior of Ti6Al4V Fabricated by Wire-Fed Electron Beam Additive Manufacturing Technology

Table 1

Composition of the Ti6Al4V materials (wt. %).

ElementAMS 4911P Ti6Al4V
3 mm thick wrought plate
AMS 4954 Ti6Al4V
0.9 mm wire

Al6.216.66
V4.004.18
Fe0.18
C0.0060.03
O0.180.18
N0.0050.007
H0.003
Y0.0050.005
TiBalanceBalance

Selected composition to compensate for evaporation of alloying elements during EBAM, especially aluminum.