Experiment scheme of electrochemical modification on the HWBM.
| Number | P (V·cm−1) | T (min) | W/C |
| 1 | 0 | 0 | 0 | 2 | 0.2 | 180 | 4 : 1 | 3 | 0.5 | 180 | 4 : 1 | 4 | 1.0 | 180 | 4 : 1 | 5 | 2.0 | 180 | 4 : 1 | 6 | 3.0 | 180 | 4 : 1 | 7 | 0.2 | 60 | 4 : 1 | 8 | 0.2 | 120 | 4 : 1 | 9 | 0.2 | 240 | 4 : 1 | 10 | 0.2 | 360 | 4 : 1 | 11 | 0.2 | 540 | 4 : 1 | 12 | 0.2 | 180 | 3 : 1 | 13 | 0.2 | 180 | 5 : 1 | 14 | 0.2 | 180 | 6 : 1 | 15 | 0.2 | 180 | 7 : 1 | 16 | 0.2 | 180 | 8 : 1 |
|
|