| Test number | Intact backfill specimens | Backfill specimens with prefabricated fracture | Remarks | Seepage water pressure (MPa) | Initial confining pressure (MPa) | Seepage water pressure (MPa) | Initial confining pressure (MPa) |
| 1 | 0 | 1.5 | 0 | 1.5 | Samples are saturated | 2 | 0.3 | 1.5 | 0.3 | 1.5 | 3 | 0.6 | 1.5 | 0.6 | 1.5 | 4 | 0.9 | 1.5 | 0.9 | 1.5 | 5 | 1.2 | 1.5 | 1.2 | 1.5 | 6 | 0.3 | 0.5 | 0.3 | 0.5 | 7 | 0.3 | 1.0 | 0.3 | 1.0 | 8 | 0.3 | 1.5 | 0.3 | 1.5 | 9 | 0.3 | 2.0 | 0.3 | 2.0 |
|
|