Experimental Study on the Creep Characteristics of Cemented Backfill in a Goaf under Water Pressure

Table 2

Creep loading scheme.

Water pressure (MPa)Axial stress (MPa)
1st level2nd level3rd level4th level5th level

03.04.05.06.07.0
0.53.04.05.06.0
1.03.04.05.06.0
1.53.04.05.0
2.03.04.05.0