The atomic and weight percentages of the mixture of Sn and oxide obtained from the EDX technique.

Calcinations temperature (°C)Sn elementO element
Weight (%)Atomic (%)Weight (%)Atomic (%)

30021.783.21
35075.9734.7617.1958.34
40078.5441.2613.0050.66
45074.3326.4618.3048.33