Research Article
Enhanced Mechanical Properties of Mg-6Sn-3Al-1Zn Alloy with Bimodal Grain Size Disturbed in the Microstructure Uniformly through Changing the Rolling Temperature
Figure 3
OM pictures of Mg-6Sn-3Al-Zn alloys rolled at different temperatures: (a) 300°C, (b) 350°C, (c) 400°C, and (d) 450°C.
(a) |
(b) |
(c) |
(d) |