Research Article
Microstructure and Conductivity of the Al-Cu Joint Processed by Friction Stir Welding
Figure 7
The fractured fracture morphology of the joints produced by (a) 750 rpm-0°, (b) 950 rpm-0°, (c) 1180 rpm-0°, (d) 1500 rpm-0°, (e) 950 rpm-2°, and (f) 1180 rpm-2°.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |