Research Article
Wear Properties of TiC-Reinforced Co50 Composite Coatings from Room Temperature to High Temperature
Table 3
Technical parameters and samples surface of the LC method applied in the experiment.
| Sample | Co50 (wt.%) | TiC (wt.%) | Laser power P (kW) | Scanning speed (mm/min) | Laser power density (kW·s/cm2) |
| S0 | 100 | 0 | 3.3 | 400 | 12.57 | S1 | 90 | 10 | 3.6 | 500 | 10.97 | S2 | 80 | 20 | 3.9 | 350 | 16.98 | S3 | 70 | 30 | 4.2 | 350 | 18.29 |
|
|